Imaging of buried archaeological materials: the reflection properties of archaeological wood

Imaging of buried archaeological materials: the reflection properties of archaeological wood
Imaging of buried archaeological materials: the reflection properties of archaeological wood
Effective marine archaeological site management demands detailed information on not only the spatial distribution of artefacts but also the degradation state of the materials present. Although sonar methods have frequently been used in an attempt to detect buried wooden shipwrecks they are currently unable to indicate their degradation state. To assess the sensitivity of acoustic measurements to changes in the degradation state of such material, and hence the potential for sonars to quantify degradation, laboratory measurements of compressional wave velocity, as well as bulk density for oak and pine samples, in varying states of decay, were undertaken. These data enabled the calculation of theoretical reflection coefficients for such materials buried in various marine sediments. As wood degrades, the reflection coefficients become more negative, resulting in the hypothesis that the more degraded wood becomes, the easier it should be to detect. Typical reflection coefficients of the order of ?0.43 and ?0.52 for the most degraded oak and pine samples in sand are predicted. Conversely, for wood exposed to seawater the predicted reflection coefficients are large and positive for undegraded material (0.35 for oak, 0.18 for pine) and decrease to zero or slightly below for the most degraded samples. This indicates that exposed timbers, when heavily degraded, can be acoustically transparent and so undetectable by acoustic methods. Corroboration of these experimental results was provided through comparison with high resolution seismic reflection data that has been acquired over two shipwrecks.
acoustics, archaeology, chirp, compressional wave velocity, reflection coefficient, shipwreck, sonar, sub-bottom profiler
0025-3235
135-144
Arnott, S.H.L.
a2e06c25-3c9c-4542-b568-69261cc6dad0
Dix, J.K.
efbb0b6e-7dfd-47e1-ae96-92412bd45628
Best, A.I.
cad03726-10f8-4f90-a3ba-5031665234c9
Gregory, D.J.
51671a5f-0435-4339-a6bc-4638efdd4cca
Arnott, S.H.L.
a2e06c25-3c9c-4542-b568-69261cc6dad0
Dix, J.K.
efbb0b6e-7dfd-47e1-ae96-92412bd45628
Best, A.I.
cad03726-10f8-4f90-a3ba-5031665234c9
Gregory, D.J.
51671a5f-0435-4339-a6bc-4638efdd4cca

Arnott, S.H.L., Dix, J.K., Best, A.I. and Gregory, D.J. (2005) Imaging of buried archaeological materials: the reflection properties of archaeological wood. Marine Geophysical Researches, 26 (2-4), 135-144. (doi:10.1007/s11001-005-3713-x).

Record type: Article

Abstract

Effective marine archaeological site management demands detailed information on not only the spatial distribution of artefacts but also the degradation state of the materials present. Although sonar methods have frequently been used in an attempt to detect buried wooden shipwrecks they are currently unable to indicate their degradation state. To assess the sensitivity of acoustic measurements to changes in the degradation state of such material, and hence the potential for sonars to quantify degradation, laboratory measurements of compressional wave velocity, as well as bulk density for oak and pine samples, in varying states of decay, were undertaken. These data enabled the calculation of theoretical reflection coefficients for such materials buried in various marine sediments. As wood degrades, the reflection coefficients become more negative, resulting in the hypothesis that the more degraded wood becomes, the easier it should be to detect. Typical reflection coefficients of the order of ?0.43 and ?0.52 for the most degraded oak and pine samples in sand are predicted. Conversely, for wood exposed to seawater the predicted reflection coefficients are large and positive for undegraded material (0.35 for oak, 0.18 for pine) and decrease to zero or slightly below for the most degraded samples. This indicates that exposed timbers, when heavily degraded, can be acoustically transparent and so undetectable by acoustic methods. Corroboration of these experimental results was provided through comparison with high resolution seismic reflection data that has been acquired over two shipwrecks.

This record has no associated files available for download.

More information

Published date: 2005
Keywords: acoustics, archaeology, chirp, compressional wave velocity, reflection coefficient, shipwreck, sonar, sub-bottom profiler

Identifiers

Local EPrints ID: 24136
URI: http://eprints.soton.ac.uk/id/eprint/24136
ISSN: 0025-3235
PURE UUID: ce82c19f-8a52-4c2f-b8d3-667eeade5a85
ORCID for J.K. Dix: ORCID iD orcid.org/0000-0003-2905-5403

Catalogue record

Date deposited: 22 Mar 2006
Last modified: 16 Mar 2024 02:45

Export record

Altmetrics

Contributors

Author: S.H.L. Arnott
Author: J.K. Dix ORCID iD
Author: A.I. Best
Author: D.J. Gregory

Download statistics

Downloads from ePrints over the past year. Other digital versions may also be available to download e.g. from the publisher's website.

View more statistics

Atom RSS 1.0 RSS 2.0

Contact ePrints Soton: eprints@soton.ac.uk

ePrints Soton supports OAI 2.0 with a base URL of http://eprints.soton.ac.uk/cgi/oai2

This repository has been built using EPrints software, developed at the University of Southampton, but available to everyone to use.

We use cookies to ensure that we give you the best experience on our website. If you continue without changing your settings, we will assume that you are happy to receive cookies on the University of Southampton website.

×