Fatigue performance of metallic beams strengthened with a bonded CFRP plate
Fatigue performance of metallic beams strengthened with a bonded CFRP plate
This paper gives details of a fatigue test programme of a series of small-scale steel beams bonded with a carbon fibre reinforced polymer (CFRP) plate. Backface-strain technique was used to detect crack initiation and monitor crack growth. Results show that this technique could detect crack initiation and track the deterioration of the adhesive layer. The strains recorded show that crack initiates and grows in Mode I earlier than in Mode II in the bonded joints, and this finding agrees with the observations on double-lap joints published in literature. The strains recorded also show that the adhesive spew fillet at the end of the CFRP plate is beneficial to the fatigue performance, although the improvement is not significant. An S–N curve was developed from the test results. The curve correlates the maximum principal interfacial stress at the plate end to the number of cycles to crack initiation. This maximum stress can be calculated from the authors’ previous analytical work. The fatigue limit of the S–N curve was found to be about 30% of the ultimate static failure stress.
CFRP plate, metallic beam, fatigue, adhesive bonding, S–N curve
222-231
Deng, J.
739ec171-0fad-4f75-89cf-01996dede033
Lee, M.K.
2a158b4e-0c01-4fd4-9cf8-99597fb3936a
April 2007
Deng, J.
739ec171-0fad-4f75-89cf-01996dede033
Lee, M.K.
2a158b4e-0c01-4fd4-9cf8-99597fb3936a
Abstract
This paper gives details of a fatigue test programme of a series of small-scale steel beams bonded with a carbon fibre reinforced polymer (CFRP) plate. Backface-strain technique was used to detect crack initiation and monitor crack growth. Results show that this technique could detect crack initiation and track the deterioration of the adhesive layer. The strains recorded show that crack initiates and grows in Mode I earlier than in Mode II in the bonded joints, and this finding agrees with the observations on double-lap joints published in literature. The strains recorded also show that the adhesive spew fillet at the end of the CFRP plate is beneficial to the fatigue performance, although the improvement is not significant. An S–N curve was developed from the test results. The curve correlates the maximum principal interfacial stress at the plate end to the number of cycles to crack initiation. This maximum stress can be calculated from the authors’ previous analytical work. The fatigue limit of the S–N curve was found to be about 30% of the ultimate static failure stress.
This record has no associated files available for download.
More information
Published date: April 2007
Keywords:
CFRP plate, metallic beam, fatigue, adhesive bonding, S–N curve
Identifiers
Local EPrints ID: 53586
URI: http://eprints.soton.ac.uk/id/eprint/53586
ISSN: 0263-8223
PURE UUID: 1ec1cbb4-8987-43b0-a8dd-caf516b3d8dc
Catalogue record
Date deposited: 22 Jul 2008
Last modified: 15 Mar 2024 10:41
Export record
Altmetrics
Contributors
Author:
J. Deng
Author:
M.K. Lee
Download statistics
Downloads from ePrints over the past year. Other digital versions may also be available to download e.g. from the publisher's website.
View more statistics