Effects of nickel-aluminum bronze pre-oxidized films on the cathodic kinetics of oxygen reduction
Effects of nickel-aluminum bronze pre-oxidized films on the cathodic kinetics of oxygen reduction
The cathodic oxygen reduction kinetics of the freshly polished and the pre-oxidized nickel-aluminum bronze surfaces were investigated in a 3.5 wt.% NaCl solution under steady-state and well-defined hydrodynamic conditions using a rotating disc electrode setup. The diffusion coefficient of the pre-oxidized film specimen of 0.72 10–5 cm2 s–1, was lower than that of the freshly polished surface of 2.55 10–5 cm2 s–1, a 3.5 fold decrease, demonstrating the extent to which the oxygen diffusion within the pre-oxidized film was hindered.
oxygen reduction kinetics, rotating disc electrode, nickel-aluminum bronze, pre-oxidized film;, oxide film
Musabikha, Siti
9abf795e-bf71-4b14-ae21-ad620db866d2
Mukhtasor, Utama
4d96a66f-ac64-4dd9-981c-cd5c58c293d3
Wharton, Julian A.
965a38fd-d2bc-4a19-a08c-2d4e036aa96b
Wood, Robert J.K.
d9523d31-41a8-459a-8831-70e29ffe8a73
Musabikha, Siti
9abf795e-bf71-4b14-ae21-ad620db866d2
Mukhtasor, Utama
4d96a66f-ac64-4dd9-981c-cd5c58c293d3
Wharton, Julian A.
965a38fd-d2bc-4a19-a08c-2d4e036aa96b
Wood, Robert J.K.
d9523d31-41a8-459a-8831-70e29ffe8a73
Musabikha, Siti, Mukhtasor, Utama, Wharton, Julian A. and Wood, Robert J.K.
(2019)
Effects of nickel-aluminum bronze pre-oxidized films on the cathodic kinetics of oxygen reduction.
Analytical Letters.
Abstract
The cathodic oxygen reduction kinetics of the freshly polished and the pre-oxidized nickel-aluminum bronze surfaces were investigated in a 3.5 wt.% NaCl solution under steady-state and well-defined hydrodynamic conditions using a rotating disc electrode setup. The diffusion coefficient of the pre-oxidized film specimen of 0.72 10–5 cm2 s–1, was lower than that of the freshly polished surface of 2.55 10–5 cm2 s–1, a 3.5 fold decrease, demonstrating the extent to which the oxygen diffusion within the pre-oxidized film was hindered.
Text
Manuscript Siti 2019 reviewed final
- Accepted Manuscript
More information
Accepted/In Press date: 1 December 2019
e-pub ahead of print date: 12 December 2019
Keywords:
oxygen reduction kinetics, rotating disc electrode, nickel-aluminum bronze, pre-oxidized film;, oxide film
Identifiers
Local EPrints ID: 437064
URI: http://eprints.soton.ac.uk/id/eprint/437064
PURE UUID: 11b86de9-6a58-46b5-96db-dceb43332ca9
Catalogue record
Date deposited: 16 Jan 2020 17:31
Last modified: 17 Mar 2024 05:15
Export record
Contributors
Author:
Siti Musabikha
Author:
Utama Mukhtasor
Download statistics
Downloads from ePrints over the past year. Other digital versions may also be available to download e.g. from the publisher's website.
View more statistics